Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RADILON S LRV150UK 333 BK - PA6-GF15 - RadiciGroup High Performance Polymers

Material Data Center offers the following functions for RADILON S LRV150UK 333 BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Radilon S datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
PA6 15% glass fibre reinforced injection moulding grade. Heat stabilized. Improved UV resistance. Black colour.

Suitable for parts requiring improved stiffness, good heat ageing resistance and which must also resist to outdoor exposure.
Механические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Модуль упругости при растяжении 6300 / - МПа ISO 527
Напряжение при разрыве 120 / - МПа ISO 527
Удлинение при разрыве 2.5 / - % ISO 527
Ударная вязкость по Шарпи, +23°C 35 / - кДж/м2 ISO 179/1eU
Ударная вязкость по Шарпи с надрезом, +23°C 5.5 / - кДж/м2 ISO 179/1eA
Теплофизические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Температура плавления, 10°C/мин 220 / * °C ISO 11357-1/-3
Класс горючести при толщине образца h HB / * класс IEC 60695-11-10
Толщина образца 0.8 / * мм -
Электрические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Удельное объемное сопротивление 1E13 / 1E11 Ом*м IEC 62631-3-1
Удельное поверхностное сопротивление * / 1E10 Ом IEC 62631-3-2
Прочие свойствасухой / кондЕдиницаСтандарт
Плотность 1240 / - кг/м³ ISO 1183
Особые свойства и характеристики
Способы переработки
Литье под давлением
Вид поставки
Мелкие гранулы, Черный
Добавки
Добавка, улучшающая съем изделия с пресс-формы
Особые показатели
Стабилизированный к УФ или погодостойкий, Термостабилизированный или стойкий к воздействию тепла
Доступность материала по регионам
Другая текстовая информация
Литье под давлением
The material is delivered in moisture-proof packaging ready for processing. Maximum recommended water content for best processing is 0.15%. Typical conditions with a desiccant drier: temperature 80 ° C, dew point -20 ° C or below, time 2-4 h or more. Special care must be taken to avoid moisture absorption and contamination with other polymers when adding regrind material. Colour variation and mechanical properties reduction may occur and should always be carefully monitored.

Injection Molding Processing Parameters
Melt Temperature Mold Temperature Injection Speed
240 - 280°C 80 - 90°C medium-high
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.